Please follow these directions for the following products to avoid leaks, clogs, and other issues. Failure to adhere to these practices may invalidate your warranty.
Leaf Filling Directions
Recommended Needle Size | Ideal Fill Temperature | Capping Time |
---|---|---|
16-20ga | 90°F/32°C (thinner oils) – 135°F/57°C (thicker oils) | 3 mins or less (depending on viscosity) |
- Insert a blunt tip 1 6 to 20g needle into the recessed holes directly next to center airway hole.
Caution: Do not allow oil to enter the center airway - 90°F/32°C (thinner oils) | 135°F/57°C (thicker oils)
The ideal fill temperature will allow for filling and capping before the oil saturates the atomizer. - Oversaturation from hot filling, thin oils, and/or slow capping will cause flooding, clogging and leaking.
- Do not overfill your devices! Fill to a maximum of 2.05mL or 1.05mL depending on your configuration. Overfilling may cause seal bulging and will force fluid through the atomizer.
- Cap within 3 minutes after filling. We recommend a shorter period of time for thinner oils. Immediately after filling, cap the device with the mouthpiece until it’s fully seated.
Leaf Capping Directions
Capping time | Capping method | Minimum capping force | Maximum capping force |
---|---|---|---|
3 mins or less (depending on viscosity) | By hand or arbor press | 9-11lbs (4-5kg) | 22lbs (10kg) |
- Make sure the mouthpiece is properly aligned and straight.
Press the mouthpiece down vertically (not at an angle) using even pressure, until you hear a click - You can seat the mouthpiece by hand, but a light-duty arbor press and jig are recommended. Do not use a hammer or mallet. Pressing at an angle can lead to damage, improper sealing, leakage, and cracking of the device
- If too much pressure (over 22lbs) is applied during capping, you can damage the device and the battery.
Check the pressure carefully. - You cannot remove the mouthpiece once it’s fully seated without damaging the device or the mouthpiece.
- Let your devices stand for between 30 minutes to 12 hours before using. During this time, the oil is priming the atomizer. More viscous oils will require more time.
NOTE: Do not use fast or high powered chargers that output more than 5v 1a. This may damage the battery.
FIFO (first in, first out) advisory:
Proper forecasting and inventory management are crucial for the best performance of battery products. Battery products that are not used within 1 year can experience battery degradation and discharge and may need to be charged before they are distributed. We recommend ensuring first-in, first-out inventory practices and not distributing battery products more than 6 months after delivery.